High-speed slide table surface strengthening
The high-speed sliding bed plate is an important part of railway turnout. The friction between the rail and the sliding bed plate is easy to cause wear during the transition of the sharp rail. The traditional composite plating process has serious pollution. Can not well meet the requirements of high-speed railway long life, safe and reliable hardness and anti-corrosion technology.


Repair Name: High Speed Sliding Table
Material name: ZG230-450


basic situation
In the long-term use of high-speed turnout sliding bed, it frequently bears pressure and friction, and it is easy to cause wear and corrosion due to the comprehensive weather environment on the railway line.


Repair requirements
1.Corrosion resistance
The protection level after 200 hours of neutral salt spray (NSS) test is not lower than the level 9 in GB / T 10125-2012.
2. Wear resistance (temporary reference hardness index hardness)
The Rockwell hardness of the coating should be HRC ≥ 40 (micro-Vickers hardness of hard chromium plating should be ≥ HV800).
3. Bonding layer strength
According to the requirements of GB / T 8165-2008, the shear strength is ≥210MPa; the internal and external bending tests should ensure that when the bending angle reaches 90 °, the bonding layer and the coating have no visible cracks.